Technical Property Chart |
|
Melting Temperature | 215oc |
Density | 1.14 - 1.16 g/cm3 |
Tensile strength at yield | 750 - 850 kg/cm3 |
Elongation at yield | 12 - 13% |
E-modulus | 24,000 to 26,300 kg/cm3 |
Hardness Rockwell 23oc | R 107 - 112 |
Durometre 23oc | D 82 - 89 |
Temperature of deflection | 80oc |
Compression Strength at yield | 940 kg/cm3 |
Notched impact strength | 5 - 11 kg cm/cm |
Impact strength at +20oc | 10 kg cm/cm |
Water absorption at 20oc | 0.3 - 3% |
Flexural strength | 1000 - 1350 kg/cm2 |
Resistance to heat (continuous) | In Air 80oc In Water 100oc In Oil 140oc |
Effect of weak acids | Resistant |
Effect of strong acids | Attacked |
Effect of weak alkalies | None |
Effect of strong alkalies | None |
Effect of Organic Solvents | Resistant to common solvents |